Paint for Steel Fabrication & Structural Steel

Fabricated steel usually leaves the workshop primed, and that primer has to hold until the topcoat goes on, sometimes weeks later on site. Marindec manufactures the primers and enamels that fabricators use, from 5L tins to 200L drums.

This page sets out which primer and topcoat suit each metal, and what the technical data sheets (TDS) say about film thickness and drying.

Structural steel coating systems

A coating system is a primer matched to the metal, plus a topcoat matched to where the steel ends up. Get the primer wrong and nothing on top of it stays put. The most common mistake is a red oxide primer on galvanised steel.

Metal and useCoating systemFrom the data sheet
Mild steel, interior or shelteredFPW15 Fast Dry Primer + Fast Dry EnamelPrimer 20–35 µm dry film thickness (DFT); enamel 20–45 µm DFT; both touch dry in about 10 minutes
Mild steel outdoors: gates, fences, framesZPPW15 anti-corrosive primer + AGRIP30+ high buildAGRIP30+ 20–45 µm DFT; next coat within 2–3 hours
Exposed steel needing a UV-stable finishTwo-pack (2K) high-build primer, ask us + 2K polyurethanePolyurethane 35–45 µm DFT; hard dry about 8 hours; full cure about 7 days
Galvanised, hot-dip galvanised and zinc-coated steelGalvanised Iron Primer + enamel topcoat50–60 µm DFT; overcoat after overnight drying
Aluminium and other non-ferrous metalsEPS15 etch primer + topcoat10–15 µm DFT; overcoat after at least 1 hour
Hot steel: flues and exhaustsHeat Resistant AluminiumContinuous dry heat up to 540 °C; no undercoat

Primers for mild steel

For most fabricated mild steel, the primer is FPW15, a fast-drying alkyd primer. Customers know the range as Armour FPW, Redox 130 or MF Red, and tenders often specify it as a red oxide primer.

ZPPW15 is the anti-corrosive grade, with a zinc-modified phosphate additive. Choose it for steel that will stand outdoors, such as gates, perimeter fencing and plant equipment.

Both go on at 20 to 35 µm DFT, are touch dry in about 10 minutes and take the topcoat within 2 hours. Airless spray is the preferred method; brush and roller suit small areas only.

Shop priming in 25L and 200L drums

In a fabrication shop, priming is a production step, so the pack size matters. FPW15 comes in 200L drums in a spray grade, a grey and a Redox 130 dipping grade.

For smaller runs there are 25L drums in grey and dark olive green, and a 5L Redox 130. ZPPW15 is listed in 25L.

For dipping, the data sheet says to bring the viscosity down to about 20 seconds in a Ford Cup 4. Thin with FD Thinner, at most 15% for air spray or brush. Hard dry takes about 4 hours, so plan stacking and loading around it.

Fast-dry enamels for quick turnaround

Fast Dry Enamel is touch dry in about 10 minutes and takes its next coat within 2 hours. That lets a part be primed and topcoated in one shift. Apply 20 to 45 µm DFT.

The spray grades, sold in 200L drums, are hard dry in about 1 hour; the standard grade takes about 4. Recoat inside the window, because fast dry enamels can wrinkle if recoated at the wrong time.

AGRIP30+ is a primer and finishing enamel in one, with an anti-corrosive additive. On clean steel it needs no undercoat unless you are building a thicker film. Colours follow the SANS colour chart and RAL.

2K polyurethane for exposed steelwork

Marindec's 2K polyurethane, Armourthane 50, is a two-pack aliphatic acrylic polyurethane finish. Its datasheet calls for a two-pack (2K) high-build primer underneath. FPW15 and ZPPW15 are single-pack alkyd primers, so use them under fast dry enamel or AGRIP30+ instead. Ask us for the 2K primer when you order the polyurethane.

Mix 7 parts base to 1 part curing agent and use it within about 4 hours at 23 °C. It is touch dry in about 3 hours and takes another coat after at least 6 hours.

It comes in 5L kits, listed in black, Light Brunswick Green H07 and Protea A58, with its own thinner. Send us the job and we'll confirm the full system before you specify it.

Galvanised and aluminium parts

Galvanised Iron Primer is made for galvanised iron, hot-dip galvanised and zinc-coated steel, where standard primers lift. It goes on at 50 to 60 µm DFT, is touch dry in about 2 hours and takes the topcoat the next day.

Aluminium and other non-ferrous metals take EPS15, a self-etching primer. It goes on thin, 10 to 15 µm DFT, and is thinned and cleaned with Standard Etch Thinner.

Fences and gates

Steel gates and perimeter fencing are among the uses the catalogue lists for FPW15-family primers, along with structural steel and plant equipment. Mild-steel fencing takes ZPPW15 and then a fast dry enamel or AGRIP30+.

Galvanised security fencing and gates take Galvanised Iron Primer first. On a repaint, scrape back loose paint, spot-prime the bare metal and topcoat the whole run.

Surface preparation and film thickness

  • Remove millscale, rust and oil. Blast exterior steel to Sa 2½ (near-white metal) and prime it the same day. See steel surface preparation.
  • Degrease with Armourphos Cleaner, and strip failed coatings with Paint Remover.
  • Paint only when the steel is dry and at least 3 °C above the dew point. Every data sheet on this page sets that condition.
  • Stripe-coat edges, welds and bolt holes by brush first, because films are thinnest there.
  • Check the wet film with a gauge as you paint. Real coverage is 50 to 70% below the data sheet figure, as the film thickness guide explains.

For a step-by-step walk-through, read how to paint structural steel.

Supply for fabricators

Marindec manufactures in Alrode, Alberton (Gauteng), for collection or delivery nationwide, with regular supply to Gauteng, Mpumalanga and the Western Cape. Primers and enamels come in 200L drums for spray and dip lines, as well as 25L and 5L packs.

See delivery and supply areas, bulk paint supply, and the systems for factories and manufacturing and mining.