| SKU | 13-500-005 |
|---|---|
| Pack sizes | 5L |
| System role | primer |
| Finish | none |
| Substrates | galvanised iron |
| Environments | interior, exterior, industrial |
| Dry time | touch ± 2 hours · hard ± 6 hours |
| Coverage | 5 m²/litre @ 70 µm DFT theoretical; practical 50 to 70% less |
| Volume solids | ± 35% |
Galvanised Iron Primer — Yellow 5L
This galvanized iron primer offers exceptional durability, corrosion resistance, and aesthetic appeal, enhancing longevity in transportation and electrical applications while improving safety, performance, and energy efficiency across multiple industries.
Use cases
- Applied to galvanised iron, hot-dip galvanised (HDG) surfaces, zinc-coated steel, pre-galvanised sheeting, security fencing, and steel gates as an adhesion primer before topcoating with enamel. Prevents paint lifting on zinc and galvanised surfaces where standard primers fail to adhere.
Technical data
From the Marindec technical data sheet for Galvprime 35 lead free galvanized iron primer (13 series), TDS 1/111010. Drying and overcoating times vary with ambient temperature.
| Type | Medium build, single pack based on modified alkyd resin with environment friendly lead free driers |
|---|---|
| Recommended film thickness | 50 to 60 µm DFT (100 to 120 µm WFT) |
| Theoretical spread rate | 5 m²/litre @ 70 µm DFT |
| Practical spread rate | 50 to 70% less than theoretical, depending on substrate & application conditions |
| Solids by volume | ± 35% |
| Touch dry @ 23 °C | ± 2 hours |
| Hard dry @ 23 °C | ± 6 hours |
| Overcoating interval | Overnight |
| Recommended thinner | Not recommended; only if required use FD Thinner. For cleaning, use FD Thinner |
| Application |
|
| Substrate conditions | Dry and free of any dirt, dust or oily residues; at least 3 °C above dew point; clean sufficiently by sandblasting or with sandpaper |
Datasheets
Frequently asked questions
What is Galvanised Iron Primer — Yellow 5L used for?
Applied to galvanised iron, hot-dip galvanised (HDG) surfaces, zinc-coated steel, pre-galvanised sheeting, security fencing, and steel gates as an adhesion primer before topcoating with enamel. Prevents paint lifting on zinc and galvanised surfaces where standard primers fail to adhere.
Which surfaces can Galvanised Iron Primer — Yellow 5L be applied to?
Suitable substrates include galvanised iron.
What thinner should I use with Galvanised Iron Primer — Yellow 5L?
Per the Marindec technical data sheet: Not recommended; only if required use FD Thinner. For cleaning, use FD Thinner.
What film thickness should Galvanised Iron Primer — Yellow 5L be applied at?
The technical data sheet recommends 50 to 60 µm DFT (100 to 120 µm WFT).
What should I know before applying Galvanised Iron Primer — Yellow 5L?
Specifically formulated for galvanised iron surfaces. Customers frequently misspell as 'galvinized iron primer' — both spellings handled in search keywords.
How quickly does Galvanised Iron Primer — Yellow 5L dry?
Per the Marindec technical data sheet: touch dry ± 2 hours and hard dry ± 6 hours at 23 °C. Drying times vary with temperature and film thickness.
What coverage does Galvanised Iron Primer — Yellow 5L give?
The Marindec technical data sheet gives a theoretical spread rate of 5 m²/litre @ 70 µm DFT. Practical spread is 50 to 70% less than theoretical, depending on substrate & application conditions.
What pack sizes are available?
Galvanised Iron Primer — Yellow 5L is supplied in 5L.